Sink Marks:
- Cause: Thick sections, insufficient packing
- Prevention: Uniform walls, proper rib ratios (50-60% of wall), adequate pack time, gas-assist for thick parts
Warpage:
- Cause: Non-uniform cooling, differential shrinkage, fiber orientation
- Prevention: Uniform wall thickness, balanced cooling, symmetric design, proper gate location
Short Shots:
- Cause: Insufficient material, inadequate flow, blocked vents
- Prevention: Proper wall thickness, adequate gating, sufficient venting, flow analysis
Weld Lines (Knit Lines):
- Cause: Converging flow fronts
- Prevention: Strategic gate placement, venting at weld locations, mold temperature optimization
Flash:
- Cause: Excessive pressure, worn tooling, inadequate clamp force
- Prevention: Proper process parameters, adequate clamp tonnage, parting line design
Burn Marks (Dieseling):
- Cause: Trapped air compressing and burning
- Prevention: Adequate venting, proper fill speed, vent placement at fill end
Voids:
- Cause: Thick sections, inadequate packing
- Prevention: Core-out thick areas, proper packing pressure/time, sequential valve gating
Jetting:
- Cause: Gate too small, too fast injection
- Prevention: Proper gate sizing, impingement design, fill speed optimization
Flow Lines:
- Cause: Varying flow speeds, temperature variations
- Prevention: Uniform flow path, consistent wall thickness, mold temperature control
Need to Know
Our plastic injection molding design process systematically addresses all potential defects through DFM review and mold flow simulation.
Key Benefits
Defect-Free Parts
Reduced Scrap
First-Time-Right Molding
Consistent Quality
Lower Production Costs
#Defects#Quality#Sink Marks#Warpage#Troubleshooting
About the Author
Q
Quality Engineering Team
Molding Quality Specialist
Published on 2024-09-15
Related Questions
What is Plastic Injection Molding Design?
What Are the Key Principles of Plastic Part Design for Injection Molding?
What Are the Key Components of Injection Mold Design?
How Does Mold Flow Analysis Improve Plastic Injection Molding Design?
What is Design for Manufacturability (DFM) in Plastic Injection Molding?